Table 1 Baseline Lesion Characteristics (QCA).

From: Compliance of a cobalt chromium coronary stent alloy – the COVIS trial

  ML Vision (n = 10) ML Zeta (n = 10)
Preprocedure reference vessel diameter (mm) 3.04 ± 0.34 2.99 ± 0.47
Preprocedure MLD (mm) 0.77 ± 0.32 0.63 ± 0.32
Preprocedure diameter stenosis (%) 73.50 ± 10.30 79.60 ± 8.80
Target vessel   
   Left anterior descending 20% 50%
   Circumflex 20% 20%
   Right coronary artery 60% 30%
Postprocedure MLD (mm) 3.34 ± 0.34 3.31 ± 0.48
Postprocedure diameter stenosis (%) 6.00 ± 1.80 5.10 ± 3.80